Standards Central

SAE-AMS5703

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 degrees F (954 degrees C) Solution, Stabilization, and Precipitation Heat Treated


General Information

Designation SAE-AMS5703
Status Active
Last Update 2019-08-14
Last Document Update None
Publisher Defense Standardization Program Office

Categories

FSG-95
    FSC-9515
Document Category
    Society of Automotive Engineers (SAE)

History

Version Date Distribution Statement Access Pages
Notice - Adoption, Tier 2 2006-03-28 A Public 1

Responsibilities

Service Organization Code
Lead Standardization Activity DLA Troop Support - Construction and Equipment Items of Supply Standardization CQ
Preparing Activity Air Force Research Laboratory (AFRL) 20
Air Force Air Force Research Laboratory (AFRL) 20
Army Army Research Laboratory, Weapons and Materials Research Directorate MR
Navy Naval Air Systems Command AS